J. ASTM Int.. October 2011, 8(9): 1–4.
Published Online: October 1, 2011
..., the KV8 is signi cantly higher than KV2. KEYWORDS: Charpy test, KV8, KV2 Introduction There are two types of strikers that can be used for the standard ISO 148-1 Charpy impact test [1]. One type of striker has a radius of 2 mm and another type of striker has a radius of 8 mm. KV2 is used to denote...